Mechanical Properties Metric English Comments
Tensile Strength, Yield 29.5 MPa
4280 psi
Crosshead speed - 2"min.; ASTM D638
LyondellBasell Alathon® M5562 High Density Polyethylene
ApplicationsALATHON M 5562 is a copolymer with medium molecular weight distribution. This resin provides moderate stiffness, toughness and stress crack resistance. Typical applications include noz..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Flint Hills 11R12A Specialty Homopolymer Polypropylene
Features: Good drop impact, radiation resistant. Product does not contain animal derived components and is phthalate-free.Applications: Injection MoldingInformation provided by Flint Hills Resour..
Tensile Strength, Yield 29.5 MPa
4280 psi
50 mm/min; ASTM D638
LG Chemical 65IH HIPS
High impact, Extrusion, Balanced mechanical properties, Good surface appearance with high gloss, Conforming to FDA CFR 177.1640, Excellent processability, Applications include refrigerator food tray..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
IRPC Polimaxx Polene 3340H Polypropylene Random Copolymer
CHARACTERISTICS: HIGH CLARITY, HIGH IMPACT, GOOD EXTRUDABILITY APPLICATIONS: BLOW MOLDING, SHEET EXTRUSION FOR COSMETIC BOTTLES, SHEET FOR THERMOFORMING, CLOSURES, FILES
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
IRPC Polimaxx Polene G2855 High Density Polyethylene
CHARACTERISTICS:GOOD IMPACT STRENGTH, MEDUIM STIFFNESSGOOD PROCESSABILITYAPPLICATIONS:BLOW MOLDINGFOR CONTAINERS FROM A FEW ml TO ABOUT 20 LITRES, LUBRICANT BOTTLES,COSMETIC BOTTLES, CHEMICAL CONTAI..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
IRPC Polimaxx Polene R1760 High Density Polyethylene
CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
JPJ Technologies PP C120 PP Copolymer Injection Molding
Information provided by JPJ Technologies
Tensile Strength, Yield 29.5 MPa
4280 psi
At 50 mm/min; ISO 527-2
Borealis Bormed™ HF840MO Polypropylene Homopolymer for Medical Applications
Bormed HF840MO is a polypropylene homopolymer intended for injection molding and is modified with an internal lubricant for products requiring a low surface friction (e.g. two-part syringes).Bormed ..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Tipco Tipcolene® FPC 20 - 20% Calcium Carbonate Reinforced Polypropylene Homopolymer
20% Calcium Carbonate Filled PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
A. Schulman POLYFORT™ FPP 809 Talc Filled Homopolymer Polypropylene
DescriptionPolyfort® FPP 809 is a 40% talc-filled homopolymer polypropylene.Information provided by A. Schulman.
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D412
ACC SMP™ EP 1009 EPI Engineered Polymers Silicone Modified Polymer
EP 1009, “Powered by Reactamine®Technology”, is a two component 100% solid Silicone Modified Polyurea with superior performance in industrial applications. EP 1009 displays extremely fast cure ti..
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D412
ACC ReactAmine® EP 350 EPI Engineered Polymers Polyurea
ReactAmine® EP-350 is a two component 100% solid Polyurea with superior performance in industrial applications. EP-350 displays extremely fast cure times with excellent adhesions to different subst..
Tensile Strength, Yield 29.5 MPa
4280 psi
At 50 mm/min; ISO 527-2
Borealis Bormed™ HD810MO Polypropylene Copolymer for Medical Applications
Bormed HD810MO is a specially modified polypropylene homopolymer intended for use in medical and medical related applications, which have to be sterilized by radiation. Products molded in HD810MO a..