Physical Properties Metric English Comments
Specific Gravity 1.45 - 1.75 g/cc
1.45 - 1.75 g/cc
Parker Chomerics CHO-SHIELD® 610 A/B Epoxy Conductive Coating
Description: CHO-SHIELD® 610 A/B is a highly conductive, two-component silver-plated-copper filled epoxy coating for application to non-conductive plastic substrates, particularly those subject to ..
Specific Gravity 1.65 - 1.75 g/cc
1.65 - 1.75 g/cc
ISO 1183
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Specific Gravity 1.60 - 1.75 g/cc
1.60 - 1.75 g/cc
ISO 1183
Raschig Group DECAL® 1760 Phenolic
Glass-fiber reinforced phenolic molding compound. Very good electrical properties, good chemical resistance and mechanical properties. This product meets the allowed upper limits for heavy metals an..
Specific Gravity 1.65 - 1.75 g/cc
1.65 - 1.75 g/cc
ISO 1183
Raschig Group DECAL® 937 Phenolic
Mica reinforced phenolic molding compound. This product meets the allowed upper limits for heavy metals and PCAs and also conforms to the requirements of the EU directives 2002/95 (RoHS), 2002/96 (W..
Specific Gravity 1.60 - 1.75 g/cc
1.60 - 1.75 g/cc
ISO 1183
Raschig Group MELOPLAS® 2500 MF
Cellulose-reinforced MF molding compound in white and colored shades. Very good electrical properties, high surface hardness, good abrasion- and UV-stability, very good resistance to chemicals - al..
Specific Gravity 1.70 - 1.75 g/cc
1.70 - 1.75 g/cc
ASTM D792
Mar-Bal MB2000-25 Thermoset Polyester Composite Molding Compound
An excellent flame and track resistant material with excellent electrical and mechanical properties. Good dielectric strength and low shrink for close dimensional control.Mar-Bal standard grades can..
Specific Gravity 1.25 - 1.75 g/cc
1.25 - 1.75 g/cc
ASTM D792
Parker Chomerics CHO-SEAL® 2532 Non-Conductive Extruded Elastomer Specifications
Description: Chomerics manufactures a dual performance extruded gasket in one simple design. By a seam vulcanization process, CHO-SEAL conductive elastomers are extruded in parallel with non-conduct..
Specific Gravity 1.70 - 1.75 g/cc
1.70 - 1.75 g/cc
ISO 12086
Isoflon ETFE
Fluoropolymer material specifications.Information provided by Isoflon.
Copyright © lookpolymers.com All Rights Reserved