Electrical Properties | Metric | English | Comments |
---|---|---|---|
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | STN IEC 60243 |
Plastcom SLOVAMID 6 GF 30 FRG 5 Polyamide 6, 30% Glass Fiber, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding, chemically reinforced with 30% glass fiber, with halogen flame retardant. Main features: flammability in accordance with UL 94 V0 at 1.6mm, glow wire at 960°C,.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Plastcom SLOVAMID 6 GF 35 FRC 5 PA6 reinforced with 35% glass fibre, with flame retardant PA 6 for injection moulding, chemically reinforced with 35 % glass fibre, with halogen free flame retardant. Main features: flammability in accordance with UL 94 V2 at 1.6 mm, glow wire at 750°C, C.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Plastcom SLOVAMID 6/66 GF 30 FRG 5 TS PA6/66, 30% glass fibre, flame retardant FeaturesPA 6 + PA 66 alloy for injection moulding, chemically reinforced with 30 % glass fibre, with halogen and phosphorus free flame retardant. Main features: flammability in accordance with UL 94.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 55 Acrylic, Injection Molding Grade Injection molding grade for very long flow paths, as well as thin-walled parts.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 66 Acrylic, Injection Molding Grade Injection molding grade used for: Fresnel lenses, filter screens for TVs and VDUs, drawing instruments.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as .. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 87 E Acrylic Grade for extruding semi-finished products such as twin-strapped panels, profile and tubes, as well as injection molding of watch glasses, dishes, bowls, water-tap hand grips and bathroom fittings, .. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 88 Acrylic Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® KR 2007/1 Acrylic Medium stiffness impact grade with good heat distortion resistance. Can be extruded to thin tubes and profile and film. Easy to vacuum form. Lamp covers, cable boxes.Data was collected by ISO met.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® KR 2014/1 Acrylic, Impact Grade High-impact grade with good mechanical properties; applications include drawing instruments, scales, containers, display stands; good processing viscosity, especially suitable for coextrusion. Extr.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | IEC 60243-1 |
PolyOne Bergamid™ B70 red RAL3001 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | ISO.243 DIN.53481 |
Omnia Plastica Akulon® PET Arnite Omnialite Arnite is a relatively new semi-crystalline polymer developed for technical applications. It is suitable for mechanical parts which require dimensional stability and a low friction coefficient. Omni.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 77 E Acrylic, Extrusion Grade Extrusion grade for semi-finished products such as profile, sheet and tubes; TV-, HiFi - and video-windows.Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® G 88 E Acrylic Same as Lucryl G 88, but higher resistance to stress cracking and higher processing viscosity. Used for: extruded protective layer on PVC, ABS and PC for outdoor applications, as well as bath tubs .. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® KR 2006/1 Acrylic, Impact Grade Impact-modified grade for highly stressed parts; highest impact and notched-impact resistance; can be mixed with general-purpose grades to get the desired toughness; highly resistant to stress crack.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® KR 2010/1 Acrylic, Impact Grade High-impact grade with good flowability (e.g. for lamp covers).Data was collected by ISO methods.Quinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | |
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
Dielectric Strength | 60.0 - 100 kV/mm | 1520 - 2540 kV/in | DIN 53481 |
Isoflon TFM Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | >= 60.0 kV/mm | >= 1520 kV/in | in air, molded; ASTM D149 |
Guarniflon PTFE G800 Polytetrafluoroethylene A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarnif.. |
|||
Dielectric Strength | >= 60.0 kV/mm | >= 1520 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 137 General Purpose Polystyrene Easy flow. Examples of Application:Injection moulding – cups and containers for the food industry, medical devices, drawing templates.Extrusion – coextrusion, high gloss surface.Synthos wa.. |
|||
Dielectric Strength | 60.0 - 80.0 kV/mm | 1520 - 2030 kV/in | Air (Tape); ASTM D149 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | Full wave impulse in oil; ASTM D3426 |
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ.. |
|||
Dielectric Strength | 60.0 - 80.0 kV/mm | 1520 - 2030 kV/in | Air (Tape); ASTM D149 |
Dalau Dalcon 001 100% Virgin PTFE Applications & Industries:General: The static and dynamic friction coefficient are numerically equal, consequently no ’Stick Slip’ occurs.Chemical: Dynamic & shaft seals; Pipes & tubing for carryi.. |
|||
Dielectric Strength | 60.0 kV/mm | 1520 kV/in | ASTM D149 |
Solvay Specialty Polymers Algoflon® A.27 PTFE (Polytetrafluoroethylene)
(discontinued **) Data provided by the manufacturer.Type IV.G.2 (except elongation at break) Classification. Suspension polymer powder grade recommended for compression molding and extrusion. PTFE possesses high iner.. |
|||
Dielectric Strength | 60.0 - 90.0 kV/mm | 1520 - 2290 kV/in | DIN 53481 |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Dielectric Strength | >= 60.0 kV/mm | >= 1520 kV/in | Grade A |
Shandong Dongyue Polymer DF-101 PTFE Molding Powder (Medium Particle Size) Usage: Can be processed to film, sheet, rob, gasket, axletree and presintered material.Packing: PTFE is packed in double layer PVC bags inside and in hard circular barrels outside.Storage: PTFE shou.. |
|||
Dielectric Strength | >= 60.0 kV/mm | >= 1520 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 171 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – biaxial-oriented sheets BOPS, XPS – lightweight insulating boards, shower enclosure panels, blends with high .. |
|||
Dielectric Strength | >= 60.0 kV/mm | >= 1520 kV/in | Transformer Oil; Ø 93x3mm; IEC 243-1 |
SYNTHOS Krasten® 172 General Purpose Polystyrene Very good heat resistance and mechanical strength. Examples of Application:Extrusion – cups for hot drinks, shower enclosure panels, lightweight XPS sheets. Blends with high impact polystyrene, SBS.. |