Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 0.500 GPa | 72.5 ksi | ASTM D638 |
Quadrant EPP TIVAR® H.O.T. UHMW-PE, Premium Heat Stabilized/Anti-Oxidant Filled, (FDA, USDA, & 3-A Dairy) (ASTM Product Data Sheet) |
|||
Tensile Modulus | 0.500 GPa @Temperature 100 °C |
72.5 ksi @Temperature 212 °F |
ISO 527 |
Solvay Specialty Polymers Amodel® AT-5001 Polyphthalamide (PPA) Resin, Dry as Molded
(discontinued **) AMODEL AT-5001 polyphthalamide resin is a neat ductile material that offers superior retention of properties after humid thermal aging, high impact at low temperature, and better mechanical properti.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 120 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 125 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA M620 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | 1.0 mm/min; ASTM D638 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | ISO 527-1/-2 |
Suzhou Hipro Polymers Hiprolon® 11ESNNHL P20 Nylon, dry Hiprolon® 11ESNNHL P20 long chain polyamide compound contains a bio-renewable resource. It features low density, low water absorbing, high dimension stability and heat stability, high cold impact.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | MD/TD; ISO 527-3 |
Borealis Bormed™ RE806CF Polypropylene Random Copolymer Bormed™ RE806CF is a random copolymer. The material is specially formulated for medical applications. Applications: Bormed™ RE806CF is recommended for medical packaging. Bormed™ RE806CF contai.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis BorPure™ RD234CF Polypropylene Random Copolymer BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | MD; ASTM D882-A |
Borealis Borstar® FB1350 Medium Density Polyethylene Borstar® FB1350 is a linear medium density polyethylene grade combining excellent extrusion properties with high film stiffness. Borstar® FB1350 is well suited for mono- and coextrusion of films .. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis RD461CF Polypropylene Random Copolymer RD461CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD461CF is recommended for food packaging, high quality stati.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa | 72.5 - 87.0 ksi | MD/TD; ISO 527-3 |
Borealis RD734CF Polypropylene Random Copolymer RD734CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD734CF is recommended for food packaging, high quality stati.. |
|||
Tensile Modulus | 0.500 GPa @Temperature 100 °C |
72.5 ksi @Temperature 212 °F |
DIN 53457 |
Zell-Metall Engineering Plastics Zellamid 1100 MO at 50% RH Improved sliding and self-lubricating properties are achieved by the addition of molybdenum disulphide. UV-radiation resistance is enhanced.Color: blackApplications: For conveyor screws |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | |
Goodfellow Polyhydroxybutyrate/Polyhydroxyvalerate (PHB 88/PHV 12) See also PHB. PHB/PHV copolymers are used in preference to PHB homopolymer for general purposes (e.g. molding containers) in order to obtain a better balance of stiffness and toughness. PHV contents.. |
|||
Tensile Modulus | 0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TS300 PA46 |
|||
Tensile Modulus | 0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-B PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-J PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TW341-N PA46 Heat Stabilized, Lubricated |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 W 20 grey 9280 PA12 Product Description: Grilamid L 20 W 20 grey 9280 is a semiflexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 grey 9280 is heat stabilized. The main featur.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 20 W 20 PA12 Product Description: Grilamid L 20 W 20 is a semi-flexible plasticized medium viscosity polyamide 12 (PA12) extrusion grade. Grilamid L 20 W 20 is heat stabilized. The main features of Grilamid L 20.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 20 Y PA12-I Product Description: Grilamid L 25 W 20 Y black 9992 is a semiflexible plasticized, medium viscosity, extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 Y black 9992 is impact modified, heat.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25 W 20 PA12 Product Description: Grilamid L 25 W 20 is a semi-flexible plasticized high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 20 is UV and heat stabilized. The main features of Grila.. |
|||
Tensile Modulus | 0.500 - 0.600 GPa @Temperature 23.0 °C |
72.5 - 87.0 ksi @Temperature 73.4 °F |
1.0 mm/min; ASTM D1708 |
Solvay Specialty Polymers Hyflon® PFA 420 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA is a family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resistance, .. |
|||
Tensile Modulus | 0.500 - 1.20 GPa | 72.5 - 174 ksi | DIN 53457 |
Isoflon ETFE Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Tensile Modulus | 0.500 GPa @Temperature 200 °C |
72.5 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TE300 PA46 Heat Stabilized |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® BM 16 nat PA* Product description: Grilon BM 16 natural is a medium viscosity multi-polyamide with a low melting point. Grilon BM 16 natural has the following features: High flexibility and toughnessVery good ori.. |
|||
Tensile Modulus | 0.500 GPa | 72.5 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® 75HF Nylon 66/6, Heat Stabilized, Conditioned Vydyne® 75HF is a medium-high-viscosity, heat-stabilized PA66/6 copolymer resin designed for extrusion applications. It is available in natural color only. Vydyne 75HF resin offers a well-balanced .. |