Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE)/Butene, Film
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of cast stretch film.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.920 g/cc
0.0332 lb/in³
ISO 1183
Melt Flow 2.2 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.2 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Stress 10.0 MPa
1450 psi
MD; ISO 527
11.0 MPa
1600 psi
TD; ISO 527
Film Elongation at Break, MD 600 %
600 %
ISO 527
Film Elongation at Break, TD 800 %
800 %
ISO 527
Elmendorf Tear Strength MD 110 g
110 g
ASTM D1922
Elmendorf Tear Strength TD 300 g
300 g
ASTM D1922
Dart Drop Test 130 g
0.287 lb
ASTM D1709
Film Tensile Strength at Break, MD 36.0 MPa
5220 psi
ISO 527
Film Tensile Strength at Break, TD 28.0 MPa
4060 psi
ISO 527
Thermal Properties Metric English Comments
Vicat Softening Point 93.0 °C
199 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 225 °C
437 °F
Copyright © lookpolymers.com All Rights Reserved