Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.0 MPa | 1600 psi | TD; ISO 527 |
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca.. |