Polymer Property : Tensile Stress = 10.0 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.0 MPa
1450 psi
MD; ISO 527
Iran Petrochemical (PCC) LL0220AA Linear Low Density Polyethylene
LL 0220 AA is a LLDPE copolymer with butene as comonomer which contains anti-oxidant. This grade is suitable for the production of blown film for light duty applications and for the production of ca..