Hexcel® HexForce™ 1168 Hybrid Composite Fabric

Category Other Engineering Material , Composite Fibers
Manufacturer Hexcel
Trade Name HexForce™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexForce™ 1168 Hybrid Composite Fabric.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hexcel features custom fabric design and manufacturing. We tailor our customers' reinforcement fabrics for optimum performance. We are able to combine two or more different fibers (carbon, glass, aramid, ceramics, Thorstrand™), to use different weaving solutions, produce preforms, etc.Information provided by Hexcel
Physical Properties Metric English Comments
Thickness 310 microns
12.2 mil
Fiber Count 2400 dtex
2160 denier
Kevlar® 49 Warp Yarn
2400 dtex
2160 denier
Kevlar® 49 Fill Yarn
Mechanical Properties Metric English Comments
Tensile Modulus 228 GPa
33000 ksi
3K Carbon Warp Yarn
228 GPa
33000 ksi
3K Carbon Fill Yarn
Descriptive Properties Value Comments
Fabric Weight (oz/yd2) 7.4
Dry
Nominal Construction (count/in) 7.25
Warp
7.25
Fill
Weave Style 2/2 Twill