Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.919 - 0.922 g/cc
0.0332 - 0.0333 lb/in³
TSTM 209 B
Melt Flow 4.0 - 5.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 - 5.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break >= 7.85 MPa
>= 1140 psi
Sheet; ASTM D882
Film Elongation at Break, MD >= 250 %
>= 250 %
ASTM D882
Elongation at Break >= 350 %
>= 350 %
Sheet; ASTM D882
Film Tensile Strength at Break, MD >= 16.67 MPa
>= 2418 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 92.0 - 94.0 °C
198 - 201 °F
ASTM D1525
Optical Properties Metric English Comments
Haze <= 12 %
<= 12 %
ASTM D1003
Gloss >= 70 %
>= 70 %
At 60°C; ASTM D523