Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Physical Properties Metric English Comments
Bulk Density 2.53 g/cc

@Temperature 1500 °C,
Time 10800 sec
0.0914 lb/in³

@Temperature 2730 °F,
Time 3.00 hour
2.71 g/cc

@Temperature 110 °C,
Time 86400 sec
0.0979 lb/in³

@Temperature 230 °F,
Time 24.0 hour
Mechanical Properties Metric English Comments
Modulus of Rupture 0.0024525 GPa

@Temperature 110 °C,
Time 86400 sec
0.35571 ksi

@Temperature 230 °F,
Time 24.0 hour
0.0067689 GPa

@Temperature 1500 °C,
Time 10800 sec
0.98176 ksi

@Temperature 2730 °F,
Time 3.00 hour
Compressive Strength 22.2 MPa

@Temperature 110 °C,
Time 86400 sec
3210 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
38.3 MPa

@Temperature 1500 °C,
Time 10800 sec
5560 psi

@Temperature 2730 °F,
Time 3.00 hour
Cold Crushing Strength
Component Elements Properties Metric English Comments
Al2O3 70 %
70 %
SiO2 10 %
10 %
Descriptive Properties Value Comments
Chemical Analysis(%),SiC+C 17
Installation Method Setting
Main Applications Slag runner
Material Required for Estimating (kg/?) 2,710