Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® SX 7012 LDPE - Blow Molding The Trithene SX 7012 resin is a low density polyethylene (LDPE) with medium molecular weight which allows the production of flasks with an adequate combination of mechanical and impact strength, fle.. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7001 LDPE - Heavy Duty Low Friction Film The Trithene TS 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and low coefficient of fricti.. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TS 7010 LDPE - Medium Duty Packaging The Trithene TS 7010 resin is a low-density polyethylene (LDPE) with a high molecular weight, excellent processability, and good mechanical properties. The incorporated additives package warrants th.. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 7001 LDPE - High Molecular Weight The Trithene TX 7001 resin is a low-density polyethylene (LDPE) with high molecular weight, designed to satisfy those applications that require high mechanical strength and environmental stress crac.. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 7010 LDPE - Medium Duty Film The Trithene® TX 7010 resin is a low-density polyethylene (LDPE) with high molecular weight, excellent processability with very good mechanical properties. Besides these properties, the material is.. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D1505 |
Iran Petrochemical (PCC) Arak 20075AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.921 g/cc | 0.0332 - 0.0333 lb/in³ | ASTM D792 |
Iran Petrochemical (PCC) Tabriz 1209AA LLDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.917 - 0.922 g/cc | 0.0331 - 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.921 - 0.923 g/cc | 0.0333 - 0.0333 lb/in³ | ASTM D1505 |
Petroquimica Triunfo Trithene® TX 7003 LDPE - Heavy Duty and Industrial Film The Trithene® TX 7003 resin is a low-density, high molecular-weight polyethylene that offers high mechanical strength and environmental stress cracking resistance (ESCR). Additionally, this product.. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | Premium Quality |
Kazanorgsintez 153-02 K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |
|||
Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | |
Kazanorgsintez 15313-003 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Density | 0.917 - 0.921 g/cc | 0.0331 - 0.0333 lb/in³ | |
Kazanorgsintez 15813-020 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Density | 0.899 - 0.923 g/cc | 0.0325 - 0.0333 lb/in³ | |
Lord Adhesives 7701 Ethyl Acetate Surface Conditioner Lord Adhesion Enhancers/Surface ModifiersTo meet the unique bonding demands that accompany the use of difficult-to-bond materials, the Lord Corporation offers a full line of adhesion enhancers/surfa.. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-01K 1st Grade Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-01K Superior Quality Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-02K 1st Grade Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-02K Superior Quality Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.887 - 0.923 g/cc | 0.0320 - 0.0333 lb/in³ | Average value: 0.908 g/cc Grade Count:23 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |