Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4020R (20405) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4020W (20425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.918 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | Base Resin; ASTM D1505 |
NIZHNEKAMSKNEFTEKHIM PE 4025W (25425) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.917 - 0.922 g/cc | 0.0331 - 0.0333 lb/in³ | TSTM 209 B |
Iran Petrochemical (PCC) Bandar Imam Poliran LH0050 LDPE
(discontinued **) Information provided by Iran Petrochemical Commercial Co. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | Premium Quality |
Kazanorgsintez 153-02 K Polyethylene Composition for Cable Industry Production Method: Composition is achieved on the basis of high pressure polyethylene (low density) and low pressure (high density) with stabilizers and other additives. Application: Composition.. |
|||
Density | 0.919 - 0.922 g/cc | 0.0332 - 0.0333 lb/in³ | |
Kazanorgsintez 15313-003 High Pressure Polyethylene Production Method: HDPE is produced by high pressure ethylene polymerization in tubular reactors. Application: Intended for production of bags, pipes, fittings, articles designed for food contac.. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-01K 1st Grade Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-01K Superior Quality Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-02K 1st Grade Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |
|||
Density | 0.9185 - 0.922 g/cc | 0.03318 - 0.0333 lb/in³ | |
Sibur 153-02K Superior Quality Polyethylene for Cable Production For application of insulation and protective coverings for wiring and cables by extrusion method. |