Tensile Strength at Break >= 7.85 MPa
>= 1140 psi
Sheet; ASTM D882
Iran Petrochemical (PCC) Bandar Imam Poliran LF0450 LDPE  (discontinued **)
Information provided by Iran Petrochemical Commercial Co.
Tensile Strength at Break >= 7.85 MPa
>= 1140 psi
Taiwan PU Corporation TPL-THANE 5085-A/B High Pressure Urethane Spraying Elastomer
5085-A is a high reactivity polyethamine content extender. 5085-B is a methylene diphenyklene dissocyanate(MDI). They make up the third generation high pressure urethane spraying elastomer. It ha..