Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) 60505 High Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 60505 High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
60505 is a HDPE injection molding grade which combines high stiffness with good physical properties. This resin is well suited for crates and toys applications.Application: crates, injection molding.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D1505
Melt Flow 5.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 16.0 MPa
2320 psi
ASTM D638
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Flexural Modulus 1.48 GPa
215 ksi
ASTM D790
Izod Impact, Notched 0.460 J/cm
0.862 ft-lb/in
ASTM D256/A
Thermal Properties Metric English Comments
Vicat Softening Point 127 °C
261 °F
ASTM D1525
Heat Distortion Temperature 78.0 °C
172 °F
ASTM D648