Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 2-3840 MO 40% Glass Filled Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
INNOPOL® CS 2-3840 MO is a 40 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-3840 MO is recommended for producing injection molded products, where the required properties are outstanding stiffness besides good impact strength.Information provided by INNO-COMP
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ISO 1183
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
nozzle diam 2.095 mm; ISO 1133
Storage Temperature <= 60.0 °C
<= 140 °F
Mechanical Properties Metric English Comments
Tensile Stress 90.0 MPa
13100 psi
50 mm/min; ISO 527-1,-2
Elongation at Yield 2.5 %
2.5 %
50 mm/min; ISO 527-1,-2
Charpy Impact, Notched 1.20 J/cm²

@Temperature -20.0 °C
5.71 ft-lb/in²

@Temperature -4.00 °F
ISO 179/1eA
1.40 J/cm²

@Temperature 23.0 °C
6.66 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 157 °C
315 °F
ISO 75-1,-2
Processing Properties Metric English Comments
Rear Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Middle Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Front Barrel Temperature 190 - 240 °C
374 - 464 °F
Injection
Melt Temperature 210 - 250 °C
410 - 482 °F
Injection
Mold Temperature 15.0 - 50.0 °C
59.0 - 122 °F
Moisture Content <= 0.070 %
<= 0.070 %
Descriptive Properties Value Comments
Resin Designation PP-B GF40
ISO 1043