Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon CP-498R Silicone Bulk Compound

Category Polymer , Thermoset , Silicone , Silicone Rubber
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon CP-498R Silicone Bulk Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.62 g/cc
0.0585 lb/in³
Silicone Property; Arlon SQA-TMS-024
Mechanical Properties Metric English Comments
Hardness, Shore A 74
74
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 5.79 MPa
840 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 130 %
130 %
Silicone Property; Arlon SQA-TMS-008
Tear Strength 15.8 kN/m
90.0 pli
Silicone Property; Arlon SQA-TMS-029
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Flammability, UL94 V-0
V-0
File E54153; 15 mil to 30 mil thickness on a substrate or carrier
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 121 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 250 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red