Processing Properties | Metric | English | Comments |
---|---|---|---|
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Start Point: 215°C |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical KEYFLEX BT 3055D Ester Type TPE Description: Injection Molding, TPC-ET, Functional, Fast Molding, Medium ModulusApplication: Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa UTPBT-HB Toughened PBT Features:High impactExcellent size stabilityEasy processingApplications:Injection moldingSwitch partsKeyboard keysE & E partsInformation Provided by Kingfa Sci. & Tech. Co., Ltd. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Injection Molding |
LG Chemical LUPOY GP5206F PC/ABS+GF20%, Flame Retardance Description: Injection Molding, PC/ABS+GF20%, Flame Retardance, General PurposeApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9, 68928-70-1, 1309-64-4 and 65997-17-3Information provided by LG.. |
|||
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 2-2130 30% Talc Filled Polypropylene Copolymer INNOPOL® CS 2-2130 is a 30 % talc-filled polypropylene compound /PP-B TD30 (ISO 1043)/. This grade is available in natural and custom colored form.INNOPOL® CS 2-2130 is recommended for produci.. |
|||
Rear Barrel Temperature | 190 - 240 °C | 374 - 464 °F | Injection |
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa MAC-701 PC/ABS Alloy Features:Excellent balance propertiesHigh impact strengthGood electro-plating propertiesGood processing propertiesApplications:Injection moldingAutomobile instrument panelElectrical and electronic p.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-G15 15% Glass Fiber Reinforced PBT Features:Good size stabilityHigh mechanical propertiesHigh heat resistanceExcellent balance propertiesApplications:Injection moldingApplication partsAuto handleDoor latchE & E partsInformation Provi.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 230°C |
Kingfa PBT-R0N Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG002 Flame Retardant PBT Features:Flame retardantGood chemical resistanceOutstanding surfaceEasy processingHigh impactApplications:Injection moldingConnectors, terminal blocksRelay, switchBobbinsPlugsE & E partsInformation .. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Start Point: 235°C |
Kingfa PBT-RG151 Flame Retardant, 15% Glass Fiber Reinforced PBT Features:Flame retardantHigh strengthHigh temperature propertiesGood electric propertiesExcellent size stabilityNo bloomingApplications:Injection moldingConnectorsRelayBobbinsPlugsE & E partsInforma.. |
|||
Rear Barrel Temperature | 210 - 240 °C | 410 - 464 °F | Injection Molding |
LG Chemical LUPOY GN5009F PC/ABS, Halogen Free Flame Retardant Description: Injection Molding, PC/ABS, Halogen Free Flame Retardant, High FlowApplication: IT/OA (Housing)CAS: 103598-77-2, 9003-56-9 and 181028-79-5Information provided by LG Chemical |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Samyang Tribit® 1503S Polybutylene Terephthalate Characteristics:High impactApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A partsAll information provided by Samyang |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 15% Mineral Filled Flame Retardant (V0). Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 30% Glass Bead Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 30% Glass Fiber Reinforced Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 220 - 240 °C | 428 - 464 °F | Aft-1. Region Temperature |
Tisan TISLAMID® 6 Flame Retardant (V0). Halogen Free Heat Stabilized Nylon 6 TISLAMID has a wide area of application in electric/electronic, automotive, durable goods and telecommunications industries. It demonstrates characteristics such as Excellent chemical resistanceElec.. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG5 PA6, 25% Glass Filled, Injection Molded BG5 is a 25% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG6H PA6, 30% Glass Filled, Injection Molded BG6 is a Heat Stabilized, 30% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | Zone 1 |
Eurostar Staramide BG4 PA6, 20% Glass Filled, Injection Molded BG4 is a 20% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN201-G10 Nylon 66 Resin 10% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN201-G20 Nylon 66 Resin 20% glass fiber reinforced, thermal resistantInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Rear Barrel Temperature | 230 - 240 °C | 446 - 464 °F | |
Beijing Chemical Industry KAIFA® MN301-G20 Nylon 66 Resin 20% glass fiber reinforced, flame retardantInformation provided by Beijing Chemical Industry Research Institute (Group) |