Ineos K50-10-136 HDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos K50-10-136 HDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished product demands outstanding physical performance. K50-10-136 combines excellent processability and environmental stress crack resistance (ESCR) with superior impact and other well-balanced end use properties.
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 500 hour
>= 500 hour
ASTM D1693A
High Load Melt Index 9.0 g/10 min
9.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Yield 25.51 MPa
3700 psi
2 in/min (50 mm/min); ASTM D638
Elongation at Break 800 %
800 %
2 in/min (50 mm/min); ASTM D638
Flexural Modulus 1.138 GPa
165.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 4.00 J/cm
7.49 ft-lb/in
Partial break; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Vicat Softening Point 132 °C
270 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Blow Molding
Region US & Canada
Bamberger Polymers Distribution