Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 25.51 MPa | 3700 psi | 2 in/min (50 mm/min); ASTM D638 |
Ineos K50-10-136 HDPE Ineos K50-10-136 is a high molecular weight, high density polyethylene copolymer. This product was developed for blowmolding automotive fuel tanks and other large parts, where the finished produc.. |