Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | >= 0.833 g/cc | >= 0.0301 lb/in³ | Packed |
Invista Polyclear® Conserve™ 1101D PET Copolymer Packaging Resin
(discontinued **) Polyclear® Conserve™ PET 1101D is a copolymer packaging resin containing 20% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve.. |
|||
Bulk Density | >= 0.833 g/cc | >= 0.0301 lb/in³ | Packed |
Invista Polyclear® Conserve™ 1101F PET Copolymer Packaging Resin
(discontinued **) Polyclear® Conserve™ PET 1101F is a copolymer packaging resin containing 10% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve.. |
|||
Bulk Density | 0.833 g/cc | 0.0301 lb/in³ | loose |
Imerys Minsilsparâ„¢ Feldspar Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys |
|||
Bulk Density | >= 0.833 g/cc | >= 0.0301 lb/in³ | |
Indorama Auriga Polymers Polyclear™ Splash 3301 PET Resin Description: Polyclear® Splash PET 3301 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.74 dl/g. Polyclear® Splash PET 3301 is designed to provide very low regenerated a.. |
|||
Bulk Density | 0.833 g/cc | 0.0301 lb/in³ | |
Green Dot Terratek® BD 4015 Biodegradable Polymer Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the.. |
|||
Bulk Density | >= 0.833 g/cc | >= 0.0301 lb/in³ | |
Indorama Auriga Polymers Invistaâ„¢ Polyclearâ„¢ Crystalâ„¢ 3302 PET Resin Description: Polyclearâ„¢ Crystalâ„¢ PET 3302 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.79 dl/g. Polyclearâ„¢ Crystalâ„¢ PET 3302 is designed to have slow re.. |
|||
Bulk Density | >= 0.833 g/cc | >= 0.0301 lb/in³ | |
Indorama Auriga Polymers Polyclear™ Refresh 1101 PET Resin Description: Polyclear® Refresh PET 1101 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Refresh PET 1101 has excellent clarity a.. |
|||
Bulk Density | 0.833 g/cc | 0.0301 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® 7000 (C91A) PET Product Description: Laser+® 7000 (C92A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typ.. |
|||
Bulk Density | 0.833 g/cc | 0.0301 lb/in³ | DAK-QAR-SOP-0018 |
DAK Americas Laser+® W 4000 K42A PET Product Description: Laser+® W 4000 (K42A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.T.. |