Chemical Properties | Metric | English | Comments |
---|---|---|---|
Carboxyl End Groups | <= 45 meq/kg | <= 45 meq/kg | Titration |
Indorama Auriga Polymers Polyclear™ Splash 3301 PET Resin Description: Polyclear® Splash PET 3301 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.74 dl/g. Polyclear® Splash PET 3301 is designed to provide very low regenerated a.. |
|||
Carboxyl End Groups | <= 45 meq/kg | <= 45 meq/kg | Titration |
Indorama Auriga Polymers Polyclear™ Perserve 2201 PET Resin Description: Polyclear® Preserve PET 2201 is designed to offer exceptional performance in hot-fill and pasteurized container applications. It has a nominal intrinsic viscosity of 0.82 dl/g. Packa.. |
|||
Carboxyl End Groups | <= 45 meq/kg | <= 45 meq/kg | Titration |
Indorama Auriga Polymers Polyclear™ Refresh 1101 PET Resin Description: Polyclear® Refresh PET 1101 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Refresh PET 1101 has excellent clarity a.. |