Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Bulk Density = 0.0301 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Packed
Invista Polyclear® Conserve™ 1101D PET Copolymer Packaging Resin  (discontinued **)
Polyclear® Conserve™ PET 1101D is a copolymer packaging resin containing 20% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve..
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Packed
Invista Polyclear® Conserve™ 1101F PET Copolymer Packaging Resin  (discontinued **)
Polyclear® Conserve™ PET 1101F is a copolymer packaging resin containing 10% post consumer recycled PET. It has a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Conserve..
Bulk Density 0.833 g/cc
0.0301 lb/in³
loose
Imerys Minsilsparâ„¢ Feldspar
Minsilspar is a 170 mesh feldspathic sand (sandspar) used primarily in the Sanitaryware industry.Information provided by Imerys
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Indorama Auriga Polymers Polyclearâ„¢ Splash 3301 PET Resin
Description: Polyclear® Splash PET 3301 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.74 dl/g. Polyclear® Splash PET 3301 is designed to provide very low regenerated a..
Bulk Density 0.833 g/cc
0.0301 lb/in³
Green Dot Terratek® BD 4015 Biodegradable Polymer
Terratek BD biodegradable composites are created from a proprietary blend of starch-based ingredients and other materials, the natural components derived from renewable grain sources account for the..
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Indorama Auriga Polymers Invistaâ„¢ Polyclearâ„¢ Crystalâ„¢ 3302 PET Resin
Description: Polyclearâ„¢ Crystalâ„¢ PET 3302 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.79 dl/g. Polyclearâ„¢ Crystalâ„¢ PET 3302 is designed to have slow re..
Bulk Density >= 0.833 g/cc
>= 0.0301 lb/in³
Indorama Auriga Polymers Polyclearâ„¢ Refresh 1101 PET Resin
Description: Polyclear® Refresh PET 1101 is a copolymer packaging resin with a nominal intrinsic viscosity of 0.83 dl/g. Packaging made from Polyclear® Refresh PET 1101 has excellent clarity a..
Bulk Density 0.833 g/cc
0.0301 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® 7000 (C91A) PET
Product Description: Laser+® 7000 (C92A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.Typ..
Bulk Density 0.833 g/cc
0.0301 lb/in³
DAK-QAR-SOP-0018
DAK Americas Laser+® W 4000 K42A PET
Product Description: Laser+® W 4000 (K42A) polyethylene terephthalate (PET) resin is a copolymer formulated for conversion to PET bottles by conventional single or two-stage processing technology.T..
Copyright © lookpolymers.com All Rights Reserved