Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Universal Wire Works 310 Stainless Steel Electrode

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Universal Wire Works
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Universal Wire Works 310 Stainless Steel Electrode.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Universal 310 electrodes were developed for the welding of 310 stainless steel. The deposited weld metal exhibits the same chemical analysis and oxidation resistance as the 310 base metal. Maintenance engineers have for years considered Alloy 310 a general purpose electrode for welding almost every analysis of carbon or alloy steels. Preheating to approximately 300 to 500 degrees F will produce strong crack-free welds in dissimilar steels. Alloy 310 is often used for welding 410, 430, and 502 in field welding where it is not possible to preheat or anneal after welding.Information provided by Universal Wire Works for their line of welding wire and filler metal.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 655 MPa
95000 psi
Elongation at Break 40 %
40 %
Component Elements Properties Metric English Comments
Carbon, C 0.12 %
0.12 %
Chromium, Cr 26.5 %
26.5 %
Iron, Fe 50.2 %
50.2 %
As Remainder
Manganese, Mn 1.8 %
1.8 %
Nickel, Ni 21 %
21 %
Silicon, Si 0.40 %
0.40 %
Users viewing this material also viewed the following: