Solvay Specialty Polymers Ajediumâ„¢ Films -- Polyetherimide Polyether Imide (PEI)

Category Polymer , Film , Thermoplastic , Polyetherimide (PEI)
Manufacturer Solvay Specialty Polymers
Trade Name Ajedium™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Ajediumâ„¢ Films -- Polyetherimide Polyether Imide (PEI).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Films of polyetherimide (PEI) are amorphous and suitable for high temperature applications. They have an excellent combination of thermal, mechanical and electrical properties, along with very low flammability and low levels of smoke evolution during combustion. These features make PEI especially well suited for electrical and electronic insulators. Applications in a variety of structural components requiring high strength and rigidity at elevated temperatures have used PEI films. Polyetherimide resists a wide range of chemicals and has good resistance to UV and gamma radiation. Its glass transition temperature allows for use at high temperatures while maintaining the high mechanical properties. Electrical properties show very good stability under variable temperatures, humidity and frequency conditions. PEI films exhibit a low dissipation factor even at very low frequencies.Features: Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Electrical Properties; High Heat Resistance; Low Smoke EmissionUses: Aircraft Interiors; Automotive Applications; Electrical/Electronic Applications; Industrial Applications; Oil/Gas ApplicationsAdditional Properties: Area Factor - 152 ft²/lb/milInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ASTM D792
Water Absorption 0.20 %

@Time 86400 sec
0.20 %

@Time 24.0 hour
ISO 62
Thickness 30.0 microns
1.18 mil
As Tested
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 103 MPa
14900 psi
ASTM D882
Film Tensile Strength at Yield, TD 107 MPa
15500 psi
ASTM D882
Film Elongation at Break, MD 99 %
99 %
ASTM D882
Film Elongation at Break, TD 140 %
140 %
ASTM D882
Film Elongation at Yield, MD 7.0 %
7.0 %
ASTM D882
Film Elongation at Yield, TD 7.0 %
7.0 %
ASTM D882
Secant Modulus, MD 2.85 GPa
413 ksi
ASTM D882
Secant Modulus, TD 2.69 GPa
390 ksi
ASTM D882
Dart Drop Test <= 80.0 g
<= 0.176 lb
ASTM D1709
Film Tensile Strength at Break, MD 114 MPa
16500 psi
ASTM D882
Film Tensile Strength at Break, TD 128 MPa
18600 psi
ASTM D882
Thermal Properties Metric English Comments
Thermal Conductivity 0.120 W/m-K
0.833 BTU-in/hr-ft²-°F
ASTM C177
Glass Transition Temp, Tg 217 °C
423 °F
DSC
Oxygen Index 47 %
47 %
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
ASTM D257
Dielectric Constant 3.15

@Frequency 1000 Hz
3.15

@Frequency 1000 Hz
ASTM D150
Dielectric Strength 33.0 kV/mm

@Thickness 0.0300 mm
838 kV/in

@Thickness 0.00118 in
ASTM D149
Dissipation Factor 0.0010

@Frequency 1000 Hz
0.0010

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Color Amber
RoHS Compliance RoHS Compliant