CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LARGE HOUSWARES, SAFETY HELMETS PACKAGINGS OF AGRICULTURE PRODUCTS, PALLETS, HEAVY DUTY ARTICLES
Physical Properties Metric English Comments
Density 0.957 g/cc
0.0346 lb/in³
ASTM D792
Environmental Stress Crack Resistance >= 9.0 hour
>= 9.0 hour
Condition B, F50; ASTM D1693
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
17.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
17.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65.5
65.5
DIN 53505
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Tensile Strength, Yield 29.5 MPa
4280 psi
ASTM D638
Elongation at Break 1000 %
1000 %
ASTM D638
Charpy Impact, Notched 0.400 J/cm²
1.90 ft-lb/in²
DIN 53453
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 200 - 260 °C
392 - 500 °F