Physical Properties Metric English Comments
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® HPS2S PC
Med/high flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, e-beam, and gamma steriliza..
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® ML7678 PC
17.5 MFR, for small, intricate parts. FDA food contact compliant in limited colors. Enhanced mold release package.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Americas regio..
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® VR2020 PC
UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-..
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX2231T PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Available in transparent and tinted colorsThis data was supplied by SABIC-IP for the Europe-Africa-..
Melt Flow 17.5 g/10 min

@Load 5.00 kg,
Temperature 190 °C
17.5 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
IRPC Polimaxx Polene R1760 High Density Polyethylene
CHARACTERISTICS: HIGH IMPACT STRENGTH, EXCELLENT SURFACE APPEARANCE, GOOD RIGIDITY CONTAIN UV STABILIZER ADDITIVEAPPLICATIONS: INJECTION MOLDING FOR CRATES, TRAYS, CASES, INDUSTRIAL PARTS, BINS, LAR..
Melt Flow 17.5 g/10 min

@Load 21.6 kg,
Temperature 190 °C
17.5 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Total MDPE HR 515 Medium Density Polyethylene, Blown Film
MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic..
Melt Flow 17.5 g/10 min

@Load 10.0 kg,
Temperature 220 °C
17.5 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ASTM D1238
Diamond Polymers ASA S-210E ASA Weatherable Polymers Extrusion Molding Grade, Medium Modulus
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 17.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
17.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Diamond Polymers Softflex® 2701-1502R
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 17.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
17.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Diamond Polymers Softflex® SF 5060 Overmold for Nylon
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 17.5 g/10 min

@Load 1.00 kg,
Temperature 235 °C
17.5 g/10 min

@Load 2.20 lb,
Temperature 455 °F
ASTM D1238
Diamond Polymers Softflex® SF 8900
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Americas region.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Asia Pacific)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Asia Pacific region.
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® ML6230 PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. Available in transparent and tinted colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle Ea..
Melt Flow 17.5 g/10 min

@Load 1.20 kg,
Temperature 300 °C
17.5 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ASTM D 1238
SABIC Innovative Plastics Lexan® SLX2231D PC Copolymer (Europe-Africa-Middle East)
Low viscosity PC copolymer blend with enhanced UV stabilization and added release agent. V2 rated. Diffusion colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.