| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.05 g/cc | 0.0379 lb/in³ | ASTM D792 |
| Melt Flow | 30 g/10 min <br>@Load 2.16 kg,<br> Temperature 230 °C |
30 g/10 min <br>@Load 4.76 lb,<br> Temperature 446 °F |
ASTM D1238 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Rockwell R | 97 | 97 | ASTM D785 |
| Tensile Strength, Yield | 27.9 MPa | 4050 psi | ASTM D638 |
| Elongation at Break | 20 % | 20 % | ASTM D638 |
| Flexural Yield Strength | 42.2 MPa | 6120 psi | ASTM D790 |
| Flexural Modulus | 2.70 GPa | 392 ksi | ASTM D790 |
| Izod Impact, Notched | 0.324 J/cm <br>@Temperature 23.0 °C |
0.606 ft-lb/in <br>@Temperature 73.4 °F |
ASTM D256 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Deflection Temperature at 0.46 MPa (66 psi) | 138 °C | 280 °F | ASTM D648 |