Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Unifrax I LLC
Trade Name Fiberfrax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Unifrax Fiberfrax® Roll Board Ceramic Fiber Paper.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The lower density, binder chemistry, and bulk ceramic fiber grade used to manufacture Fiberfrax Rollboard paper result in a product with lower cost, higher flexibility, and reduced smoke and odor during burnout. Rollboard paper is best suited for wrapping intricate shapes or molds and as a standard grade single use product in disposable applications.Information Provided by Unifrax I LLC
Physical Properties Metric English Comments
Density 0.160 g/cc
0.00579 lb/in³
Loss On Ignition 3.0 %
3.0 %
including binder
Mechanical Properties Metric English Comments
Tensile Strength at Break 0.152 MPa
22.0 psi
As manufactured
Tensile Strength, Yield 0.400 MPa
58.0 psi
As manufactured
Compressive Strength 0.00689 MPa
1.00 psi
10% deformation
0.0345 MPa
5.00 psi
25% deformation
0.221 MPa
32.0 psi
50% deformation
Thermal Properties Metric English Comments
Melting Point 1760 °C
3200 °F
Maximum Service Temperature, Air 1100 °C
2010 °F
Recommended Operating Temperature
Component Elements Properties Metric English Comments
Al2O3 47 - 52 %
47 - 52 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 48 - 53 %
48 - 53 %
Descriptive Properties Value Comments
Color Off-White
Fiber Index (% Wt) 40
Na2O3 (%) <0.5
Temperature Grade (°C) 1260