SK Chemicals SKYTHANE® 310 Hotmelt Grade UB Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer SK Chemicals
Trade Name SKYTHANE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SK Chemicals SKYTHANE® 310 Hotmelt Grade UB Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical property. It is widely used for automotive parts and various industrial parts.Information provided by SK Chemicals
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Strength, Ultimate 41.2 MPa
5970 psi
ASTM D412
Tensile Strength, Yield 4.61 MPa

@Strain 100 %
668 psi

@Strain 100 %
ASTM D412
5.39 MPa

@Strain 300 %
782 psi

@Strain 300 %
ASTM D412
Elongation at Break 900 %
900 %
ASTM D412
Tear Strength 83.4 kN/m
476 pli
ASTM D624
Thermal Properties Metric English Comments
Melting Point 69.0 °C
156 °F
ASTM D3418
Softening Point 120 °C
248 °F
Ring & Ball; ASTM E28
Users viewing this material also viewed the following: