Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.324 J/cm | 0.606 ft-lb/in | ASTM D256 |
Kolon DIAMAT® IM Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Izod Impact, Notched | 0.324 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.606 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical Lupox® DP1000DU PBT Description: Injection Molding, PBT, General PurposeCAS No. 30965-26-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PD701 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PD943 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.324 J/cm | 0.607 ft-lb/in | ASTM D256A |
Lotte Chemical Titan TITANPRO® PM201 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Izod Impact, Notched | 0.324 J/cm @Temperature 23.0 °C |
0.606 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
IRPC Polimaxx Polene 2311SCX TA4 Polypropylene Compound CHARACTERISTICS: POLYPROPYLENE BLOCK COPOLYMER WITH 20% TALCUM REINFORCED GOOD IMPACT STRENGTH, HIGH FLOWAPPLICATIONS: INJECTION MOLDING FOR AUTOPARTS, ELECTRICAL APPLIANCES |
|||
Izod Impact, Notched | 0.324 J/cm | 0.606 ft-lb/in | |
Shinil Chemical SHINSTRA PA-66 W100SRB Structural Polymer Abrasion Resistance SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog.. |
|||
Izod Impact, Notched | 0.324 J/cm | 0.606 ft-lb/in | ASTM D256 |
Cheng Yu Plastic FV30720 POM, 20% Mineral Reinforced |
|||
Izod Impact, Notched | 0.324 J/cm @Thickness 3.20 mm, Temperature 23.0 °C |
0.606 ft-lb/in @Thickness 0.126 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |