Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Rexell® H2104 Injection Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Rexell® H2104 Injection Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.aInformation provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Viscosity 42 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
42 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
73 cP

@Shear Rate 1000 1/s,
Temperature 230 °C
73 cP

@Shear Rate 1000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
102 cP

@Shear Rate 300 1/s,
Temperature 230 °C
102 cP

@Shear Rate 300 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Melt Flow 34 g/10 min
34 g/10 min
Melt Flow Ratio (I10/I2) is 7.3; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 67
67
ASTM D2240
Tensile Strength, Ultimate 10.0 MPa
1450 psi
ASTM D638
Tensile Strength, Yield 22.0 MPa
3190 psi
ASTM D638
Elongation at Break 100 %
100 %
ASTM D638
Modulus of Elasticity 1.262 GPa
183.0 ksi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 121 °C
250 °F
ASTM D1525