Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 102 cP @Temperature 45.0 °C |
102 cP @Temperature 113 °F |
|
BASF Pluracol® 1135i Specialty Polyol Description: Pluracol® 1135i polyol is a nominal 1500 molecular weight triol. Pluracol 1135i has been prepared for applications in flexible slabstock foams and polyurethane adhesive and sealants ap.. |
|||
Viscosity | 102 cP @Temperature 70.0 °C |
102 cP @Temperature 158 °F |
|
BASF Pluracol® 3042 Specialty Polyol Description: Pluracol® 3042 polyol is 41 hydroxyl number (nominal 4000 molecular weight) propoxylated polyether.Information provided by BASF |
|||
Viscosity | 102 cP @Shear Rate 300 1/s, Temperature 230 °C |
102 cP @Shear Rate 300 1/s, Temperature 446 °F |
Apparent viscosity; ASTM D3835 |
Huntsman Rexell® H2104 Injection Molding LLDPE
(discontinued **) Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15.. |