Modulus of Elasticity 1.262 GPa
183.0 ksi
ASTM D638
Huntsman Rexell® H2104 Injection Molding LLDPE  (discontinued **)
Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15..