Physical Properties Metric English Comments
Viscosity 42 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
42 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Huntsman Rexell® H2104 Injection Molding LLDPE  (discontinued **)
Linear-low high density homopolymer, injection molding, FDA compliant.Features: High flow and short cycle times.Applications: Thin wall containers.FDA Notes: Conforms to FDA regulation 21 CFR 177.15..