Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Rexell® H2103 Injection Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Rexell® H2103 Injection Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage caps.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)3.2.aInformation provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Viscosity 66 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
66 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
144 cP

@Shear Rate 1000 1/s,
Temperature 230 °C
144 cP

@Shear Rate 1000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
228 cP

@Shear Rate 300 1/s,
Temperature 230 °C
228 cP

@Shear Rate 300 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Melt Flow 10.7 g/10 min
10.7 g/10 min
Melt Flow Ratio (I10/I2) is 7.7; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 64
64
ASTM D2240
Tensile Strength, Ultimate 11.0 MPa
1600 psi
ASTM D638
Tensile Strength, Yield 19.0 MPa
2760 psi
ASTM D638
Elongation at Break 200 %
200 %
ASTM D638
Modulus of Elasticity 0.938 GPa
136 ksi
ASTM D638
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
ASTM D1525