Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10.7 g/10 min @Load 1.20 kg, Temperature 300 °C |
10.7 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® ML7647 PC (Asia Pacific) Non FR Impact modified PC, excellent Fatigue performance with balanced Flow and impact. Available in Opaque only |
|||
Melt Flow | 10.7 g/10 min | 10.7 g/10 min | Melt Flow Ratio (I10/I2) is 7.7; ASTM D1238 |
Huntsman Rexell® H2103 Injection Molding LLDPE
(discontinued **) Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage .. |
|||
Melt Flow | 10.7 g/10 min @Load 3.80 kg, Temperature 230 °C |
10.7 g/10 min @Load 8.38 lb, Temperature 446 °F |
|
Arkema Group Oroglas® SG 7 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 7 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no adverse .. |