Mechanical Properties Metric English Comments
Modulus of Elasticity 0.938 GPa
136 ksi
ASTM D638
Huntsman Rexell® H2103 Injection Molding LLDPE  (discontinued **)
Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage ..