Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Elasticity | 0.938 GPa | 136 ksi | ASTM D638 |
Huntsman Rexell® H2103 Injection Molding LLDPE
(discontinued **) Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage .. |