Physical Properties Metric English Comments
Viscosity 66 cP

@Shear Rate 5000 1/s,
Temperature 230 °C
66 cP

@Shear Rate 5000 1/s,
Temperature 446 °F
Apparent viscosity; ASTM D3835
Huntsman Rexell® H2103 Injection Molding LLDPE  (discontinued **)
Linear-low medium density homopolymer, injection molding, FDA compliant.Features: Good ESCR, low taste and order.Applications: Containers, closures, and ideal for blends and non-carbonated beverage ..