Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman CP808-01 Natural Linear, Low-Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionCP 808-01 is a lineal low-density polyethylene having good processability and exceptional toughness in injection molded parts. This compound has excellent flexibility, high impact strength, excellent stress crack resistance, and good gloss. ApplicationCP 808-01 meets the specification contained in FDA Regulation 21CFR177.1520(c)3.1.Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.924 g/cc
0.924 g/cc
ASTM D792
ESCR 100% Igepal® 250 hour
250 hour
Condition C; ASTM D1693
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Condition E; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 45
45
ASTM D2240
Tensile Strength, Yield 11.0 MPa
1600 psi
2"/min; ASTM D638
Elongation at Break 175 %
175 %
2"/min; ASTM D638
Flexural Modulus 0.317 GPa
46.0 ksi
at 1% secant modulus; ASTM D790
Falling Dart Impact 28.5 J

@Temperature -40.0 °C
21.0 ft-lb

@Temperature -40.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Brittleness Temperature -68.0 °C
-90.4 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 122 °C
252 °F
Users viewing this material also viewed the following: