Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, and bundling.FDA Notes: Conforms to FDA regulation 21 CFR 177.1520 (c)2.2 under condition of use B through H described in Table 2 of 21 CFR 176.170Film properties based on 1.0 guage (25 µm) thickness; blow-up ratio 2:1.Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.924 g/cc
0.0334 lb/in³
ASTM D1505
Thickness 25.4 microns
1.00 mil
Melt Flow 0.80 g/10 min
0.80 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
ASTM D2240
Tensile Strength, Ultimate 14.0 MPa
2030 psi
ASTM D638
Tensile Strength, Yield 10.0 MPa
1450 psi
ASTM D638
Film Elongation at Break, MD 150 %
150 %
ASTM D882
Film Elongation at Break, TD 500 %
500 %
ASTM D882
Elongation at Break 650 %
650 %
ASTM D638
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Secant Modulus, MD 0.238 GPa
34.5 ksi
ASTM D882
Secant Modulus, TD 0.276 GPa
40.0 ksi
ASTM D882
Dart Drop 3.54 - 3.94 g/micron
90.0 - 100 g/mil
ASTM D1709
Dart Drop Test 90.0 - 100 g
0.198 - 0.221 lb
ASTM D1709
Film Tensile Strength at Break, MD 22.0 MPa
3190 psi
ASTM D882
Film Tensile Strength at Break, TD 21.0 MPa
3050 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Optical Properties Metric English Comments
Gloss 45 %
45 %
at 45°; ASTM D523
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F