Polymer Property : Secant Modulus, TD = 0.276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Secant Modulus, TD 0.276 GPa
40.0 ksi
ASTM D882
Chevron Phillips 6109FK Linear low density polyethylene blown film resin  (discontinued **)
Resin Type: linear low density polyethylene, butene copolymer, medium antiblock, medium slip, process aid version of 6109, blown film resinCharacteristics: good stiffness at thin gauges, good drawdo..
Secant Modulus, TD 0.276 GPa
40.0 ksi
ASTM D882
ExxonMobil Escorene® LL-3113 LLDPE/Hexene Premium High Strength, 0.7 mil Film  (discontinued **)
Data provided by the manufacturer, Exxon Chemical.An LLDPE hexene copolymer film resin. Films made from this resin have outstanding tensile, stiffness and toughness properties. These superior prope..
Secant Modulus, TD 0.276 GPa
40.0 ksi
0.01; ASTM D882
Westlake Hifor SC74561-F Clear (Voridian) Polyethylene Film, Using Energx Technology Services  (discontinued *
VORIDIAN HIFOR CLEAR SC74558-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and low antiblock additives. Films produced with t..
Secant Modulus, TD 0.276 GPa
40.0 ksi
ASTM D882
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Secant Modulus, TD 0.276 GPa
40.0 ksi
1% Secant; ASTM D882
Westlake Hifor SC74560-F Clear Polyethylene  (discontinued **)
Hifor Clear Polyethylene SC74560-F polymer is a high strength and high clarity polyethylene designed for blown film extrusion that contains medium slip and medium antiblock additives. Films produc..