Polymer Property : Modulus of Elasticity = 0.276 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE 1008 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: industrial packaging, frozen food, produce bags, shrink, a..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE1031 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Superior strength, good machinability, and heat seal characteristics.Applications: Film extrusion: clarity packaging, frozen food, produce bags, shrink, bund..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE1033 Film Extrusion Polyethylene  (discontinued **)
Homopolymer, and FDA compliant.Features: Good opticals, impact strength, good processing properties, and stiffnessApplications: Film extrusion: general purpose packaging and film applications.FDA No..
Modulus of Elasticity 0.276 - 0.703 GPa
40.0 - 102 ksi
ASTM D638M
DSM Somos® 8120 Epoxy Photopolymer  (discontinued **)
DescriptionDSM Somos® 8120 is a high-speed liquid photopolymer that produces flexible, high-impact-strength, accurate parts using stereolithography machines. It has a wide processing latitude and ..
Modulus of Elasticity 0.276 - 0.700 GPa
40.0 - 102 ksi
Average value: 0.454 GPa Grade Count:8
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE1061 Film Extrusion Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Exceptional strength, good machinability and heat seal characteristics.Applications: Film extrusion: high clarity packaging, frozen food, produce bags, shrink..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE2060 Injection Molding Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: High flow characteristics, good processability.Applications: Injection molding: general purpose molding, large moldings including housewares and toys.FDA Note..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE6010 Blow Molding Polyethylene  (discontinued **)
Homopolymer, Drug Master File listed product, complies with USP Classification VI, and FDA compliant.Features: Meets exacting requirements of blow molded containers and processes well with parison s..
Modulus of Elasticity 0.276 GPa
40.0 ksi
Secant; ASTM D638
Huntsman PE8010 Specialty Polyethylene  (discontinued **)
Homopolymer and FDA compliant.Features: Yields film with excellent draw down and machinability.Applications: Film extrusion: gel free film applications.FDA Notes: Conforms to FDA regulation 21 CFR 1..