Guarniflon PTFE G300 Polytetrafluoroethylene

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , Polytetrafluoroethylene (PTFE), Extruded
Manufacturer Guarniflon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Guarniflon PTFE G300 Polytetrafluoroethylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A virgin PTFE with low coefficient of friction, excellent chemical inertness, non-adhesive surface, wide service temperature range, and excellent dielectric propertiesInformation provided by Guarniflon®
Physical Properties Metric English Comments
Density 2.13 - 2.20 g/cc
0.0770 - 0.0795 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength >= 18.0 MPa
>= 2610 psi
extruded; ASTM D1708
Elongation at Break >= 180 %
>= 180 %
extruded; ASTM D1708
Compressive Yield Strength 4.00 - 6.00 MPa

@Strain 1.00 %
580 - 870 psi

@Strain 1.00 %
ASTM D695
Coefficient of Friction, Dynamic 0.060
0.060
ASTM D1894
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -200 °C
-328 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 20.0 kV/mm
>= 508 kV/in
in air; ASTM D149