Material Notes:
Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also available in gunning variety, marked "GM".Information provided by Gouda Vuurvast.
Physical Properties Metric English Comments
Bulk Density 0.810 - 0.890 g/cc
0.0293 - 0.0322 lb/in³
After drying at 110°C
Particle Size <= 5000 µm
<= 5000 µm
Grain Size
Mechanical Properties Metric English Comments
Compressive Strength 1.20 - 1.80 MPa

@Temperature 1000 °C
174 - 261 psi

@Temperature 1830 °F
Cold Crushing Strength
1.70 - 2.30 MPa

@Temperature 100 °C
247 - 334 psi

@Temperature 212 °F
Cold Crushing Strength
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 - 0.270 W/m-K

@Temperature 100 °C
1.32 - 1.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
0.230 - 0.310 W/m-K

@Temperature 600 °C
1.60 - 2.15 BTU-in/hr-ft²-°F

@Temperature 1110 °F
0.250 - 0.330 W/m-K

@Temperature 1000 °C
1.74 - 2.29 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Maximum Service Temperature, Air 1250 °C
2280 °F
Shrinkage -0.400 - 0.400 %

@Temperature 1000 °C
-0.400 - 0.400 %

@Temperature 1830 °F
Permanent Linear Change
Component Elements Properties Metric English Comments
Al2O3 33 %
33 %
Fe2O3 1.0 %
1.0 %
SiO2 55 %
55 %
Descriptive Properties Value Comments
ASTM Classification Q
Material Consumption per 1 m3 780 kg
Mixing Water 45-55 liters
per 100 kgs dry material
Users viewing this material also viewed the following: