Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 0.190 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 W/m-K

@Temperature 100 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 212 °F
(DIN 51046)+
Pyrotek Pyrite B-3 Refractory Board
Pyrotek B-3 is a highly versatile calcium silicate board for use in a variety of machined shapes and general purpose applications. Among its uses, Pyrotek B-3 is established as the industry standar..
Thermal Conductivity 0.190 W/m-K

@Temperature 815 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Pyrotek Thermollite Insulating Refractory Shapes for Molten Aluminum
Thermollite has been specifically developed for direct contact with molten aluminum and its various alloys. Thermollite provides the specific advantage of reducing heat loss in melt transfer applic..
Thermal Conductivity 0.190 W/m-K

@Temperature 800 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.190 W/m-K

@Temperature 50.0 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 122 °F
DuPont Performance Polymers Kalrez® 1058 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that has been plasticized with perfluorinated oil. It is the softest, lowest modulus compound in the Kalrez line. Generally it is similar in resistance to Compound 1..
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 600 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GI 23 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 100 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va..
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 600 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 135 L Refractory Insulating Castable
Description: Golite 135 L can be used in direct contact with fire and combines a good strength with a high insulation value.Remarks: These values apply to cast products. Also available in gunning va..
Thermal Conductivity 0.190 W/m-K

@Temperature 982 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1800 °F
Mid-Mountain Materials CERMEX® PR1800SW Low Biopersistence Thermal Insulation Paper
Material: Alkaline Earth Silicate Wool Construction: Paper, Organic BinderInformation provided by Mid-Mountain Materials
Thermal Conductivity 0.190 - 0.290 W/m-K

@Temperature 100 °C
1.32 - 2.01 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 120 Refractory Insulating Castable
Description: Golite 120 is composed of light weight aggregates, alumina cement and special additions to be sure of a high strength and a low firing shrinkage.Remarks: These values apply to cast prod..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group Moler LR-1750 Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group SKAMOLEX V-1100 (475) Customized Shape
SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group SKAMOLEX V-1100 (600) Customized Shape
SKAMOLEX customized shapes have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulationA large variety of specialized and vers..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group V-1100 475 Vermiculite Insulating Slab
SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C-182
Skamol Group V-LITE 475 Vermiculite Insulating Brick
V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica..
Thermal Conductivity 0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
Thermal Ceramics Cerablanket Blanket
Cerablanket is produced from exceptionally pure oxides of alumina and silica using the spinning process. The resultant quality spun fibers have been optimized for high handling strength, with on ave..
Thermal Conductivity 0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
4 pcf
Thermal Ceramics Cerachrome Blanket
Made from spun alumina-silica-chromia fiber, Cerachrome Blanket is well suited for hot face lining applications where higher temperatures are encountered, such as soaking pit covers, reheat and forg..
Thermal Conductivity 0.190 W/m-K

@Temperature 1075 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1967 °F
Parallel to thickness; ASTM C177-76
Zircar Ceramics AL-30 Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.190 W/m-K

@Temperature 1100 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 2010 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ALC Alumina Insulation
ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics.
Thermal Conductivity 0.190 W/m-K

@Temperature 1400 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.190 W/m-K

@Temperature 1400 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYFB-3 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.190 W/m-K

@Temperature 800 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.190 W/m-K

@Temperature 1400 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYZ-3 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Zircar Ceramics APA-3 Alumina Paper
ZIRCAR Alumina Papers are uniform structures made principally of alumina fiber. APA-3 is a thin uniformly rigidized sheet of alumina fiber and binder. Applications include thermal insulation in lo..
Thermal Conductivity 0.190 W/m-K

@Temperature 538 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1000 °F
ASTM C182
BNZ Materials BNZ-23 Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.190 W/m-K

@Temperature 600 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1110 °F
ASTM C182
BNZ Materials BNZP-23L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.190 W/m-K

@Temperature 1400 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYC Zirconia Cylinders Insulation
Zircar Zirconia Cylinders Type ZYC are rigid, free standing refractory structures composed of yttria stabilized zirconia fibers that are bonded with silica. The material is evenly bonded, allowing ..
Thermal Conductivity 0.190 W/m-K

@Temperature 1075 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 1967 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics AL-30AA Alumina Insulation
AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C..
Thermal Conductivity 0.190 W/m-K

@Temperature 50.0 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 122 °F
DuPont Performance Polymers Kalrez® 4079 FFKM Perfluoroelastomer
A low compression set compound for general-purpose use in O-rings, diaphragms, seals, and other parts used in the process and aircraft industries. It is a carbon black-filled compound with excellen..
Thermal Conductivity 0.190 W/m-K

@Temperature 315 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 599 °F
Pyrotek ISOMAG® 45 Thermal Insulation Board
Isomag® 45 is a medium density insulating board which provides excellent hot strength and insulating value. Its magnesia silicate based formulation provides insulating properties equivalent to cal..
Thermal Conductivity 0.190 W/m-K

@Temperature 50.0 °C
1.32 BTU-in/hr-ft²-°F

@Temperature 122 °F
DuPont Performance Polymers Kalrez® 3018 FFKM Perfluoroelastomer  (discontinued **)
A carbon black-filled compound that is similar to Compound 1050LF, except for higher hardness/modulus. Best hot water/steam resistance. Generally used in oil fields and process industry application..
Copyright © lookpolymers.com All Rights Reserved