Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.250 W/m-K @Temperature 815 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 1500 °F |
|
Pyrotek SF-50 Foamed Fused Silica Insulation Board SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1400 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.250 - 0.350 W/m-K @Temperature 1000 °C |
1.74 - 2.43 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GI 23 Insulating Refractory Brick This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast. |
|||
Thermal Conductivity | 0.250 - 0.330 W/m-K @Temperature 600 °C |
1.74 - 2.29 BTU-in/hr-ft²-°F @Temperature 1110 °F |
|
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th.. |
|||
Thermal Conductivity | 0.250 - 0.330 W/m-K @Temperature 1000 °C |
1.74 - 2.29 BTU-in/hr-ft²-°F @Temperature 1830 °F |
|
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 400 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 752 °F |
ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group SKAMOCAST 14-105 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 200 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 392 °F |
Mean temp.; ASTMÂ C-201 supplemented by ASTM C-182 |
Skamol Group VERMICAST 14-100 Insulating Castable SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 800 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 1470 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1350 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2460 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1400 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1400 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 816 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 1500 °F |
ASTM C182 |
BNZ Materials BNZ-23HS Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1000 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 1830 °F |
ASTM C182 |
BNZ Materials BNZP-23L Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1350 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2460 °F |
Parallel to Thickness; ASTM C177-76 |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 1400 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 2550 °F |
|
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo.. |
|||
Thermal Conductivity | 0.250 W/m-K @Temperature 23.0 °C |
1.74 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
|
Touchstone CFOAM® 20 Structural Carbon Foam CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins.. |