Total ESD 201 B HDPE blow molding

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Total Atofina
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Total ESD 201 B HDPE blow molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FINATHENE® ESD 201 B is a black conductive compound manufactured from high performance Finathene high density polyethylene. The use of this HDPE compound gives outstanding compatibility to (semi) high molecular weight, high density polyethylene and assures smooth processing on typical machines used in the industry. FINATHENE® ESD 201B has been developed for the production of high performance industrial parts, intended for use in explosive/hazardous atmospheres.Information provided provided by Total Petrochemicals.Total Petrochemicals acquired former Fina and Atofina plastics product lines.
Physical Properties Metric English Comments
Density 0.995 g/cc
0.0359 lb/in³
ISO 1183
Environmental Stress Crack Resistance >= 250 hour
>= 250 hour
ASTM D1693-70
Melt Flow 4.5 g/10 min

@Temperature 190 °C
4.5 g/10 min

@Temperature 374 °F
High Load; ISO 1133
Mechanical Properties Metric English Comments
Flexural Modulus 1.20 GPa
174 ksi
ISO 178
Electrical Properties Metric English Comments
Volume Resistivity <= 10000 ohm-cm
<= 10000 ohm-cm
Surface Resistance <= 10000 ohm
<= 10000 ohm