Polymer Property : Thermal Conductivity = 0.270 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.190 - 0.270 W/m-K

@Temperature 100 °C
1.32 - 1.87 BTU-in/hr-ft²-°F

@Temperature 212 °F
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable
Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa..