Polymer Property : Thermal Conductivity = 0.250 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.250 W/m-K

@Temperature 815 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 1500 °F
Pyrotek SF-50 Foamed Fused Silica Insulation Board
SF-50 is characterized by its uniform open cell structure which allows it to be machined to close tolerances. It can be drilled, sawed or modified with conventional tools. For quick construction o..
Thermal Conductivity 0.250 W/m-K

@Temperature 1400 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.250 - 0.350 W/m-K

@Temperature 1000 °C
1.74 - 2.43 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GI 23 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Thermal Conductivity 0.250 - 0.330 W/m-K

@Temperature 600 °C
1.74 - 2.29 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast GOLITE 1.2.4. Mix Refractory Insulating Castable
Description: This lightweight castable is composed of 1 part cement, 2 parts light weight grains and 4 parts vermiculite. Special additives provide for higher strength and less shrinkage.Remarks: Th..
Thermal Conductivity 0.250 - 0.330 W/m-K

@Temperature 1000 °C
1.74 - 2.29 BTU-in/hr-ft²-°F

@Temperature 1830 °F
Gouda Vuurvast GOLITE 125 R Refractory Insulating Castable
Description: Golite 125 R has a low Fe2O3 content and a very low density. Commonly used in reducing conditions in the petrochemical industry.Remarks: These values apply to cast products. Also availa..
Thermal Conductivity 0.250 W/m-K

@Temperature 400 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 752 °F
ASTM C-201 supplemented by ASTM C-182
Skamol Group SKAMOCAST 14-105 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Thermal Conductivity 0.250 W/m-K

@Temperature 200 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-201 supplemented by ASTM C-182
Skamol Group VERMICAST 14-100 Insulating Castable
SKAMOL insulating castables have the following characteristics: Max. service temperature: Up to 1100°C (2102°F)Back-up insulation or hot-face usesFor casting and gunningProducts are based on f..
Thermal Conductivity 0.250 W/m-K

@Temperature 800 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 1470 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics SALI-2 Alumina Insulation
SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics.
Thermal Conductivity 0.250 W/m-K

@Temperature 1350 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2460 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15AA Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.250 W/m-K

@Temperature 1400 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYFB-6 Zirconia Boards, Discs, and Cylinders Insulation
Type ZYFB Boards, Discs and Cylinders are rigid, refractory structures composed of yttria-stabilized zirconia fibers that do not undergo the usual phase transitions associated with pure zirconia. Ty..
Thermal Conductivity 0.250 W/m-K

@Temperature 1400 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.250 W/m-K

@Temperature 816 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 1500 °F
ASTM C182
BNZ Materials BNZ-23HS Insulating Firebrick
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.250 W/m-K

@Temperature 1000 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 1830 °F
ASTM C182
BNZ Materials BNZP-23L Insulating Firebrick (French Grade)
BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem..
Thermal Conductivity 0.250 W/m-K

@Temperature 1350 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2460 °F
Parallel to Thickness; ASTM C177-76
Zircar Ceramics ZAL-15 Alumina Insulation
ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics.
Thermal Conductivity 0.250 W/m-K

@Temperature 1400 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 2550 °F
Zircar Zirconia ZYZ-6 Zirconia Boards and Discs Insulation
Type ZYZ Boards and Discs are rigid, refractory structures composed of yttria-stabilized zirconia fibers that are bonded with silica. This unique composition provides Type ZYZ insulation with the lo..
Thermal Conductivity 0.250 W/m-K

@Temperature 23.0 °C
1.74 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Touchstone CFOAM® 20 Structural Carbon Foam
CFOAM, developed by Touchstone Research Laboratory, Ltd., is a next generation structural material which is inexpensive, lightweight, fire-resistant, impact-absorbing, and which can be thermally ins..